Journal Articles
Alloy Digest (2013) 62 (8): Fe-161.
Published: 01 August 2013
... coercive force glass-sealing applications hardness heat treatability magnetic permeability nonmetallic inclusions physical properties Sandvik Safeni 52 tensile properties thermal expansion workability UNS N14052 DATA ON WORLDWIDE METALS AND ALLOYS Copyright Ā© 2013, ASM InternationalĀ®. All...
Journal Articles
Alloy Digest (2006) 55 (3): Fe-138.
Published: 01 March 2006
... joinability physical properties tensile properties workability thermal properties UNS K93601, K94100, N14052 (Nominal) Ni36 Ni42 Ni52 Carbon 0.01 Manganese 0.30 0.40 0.30 Silicon 0.20 0.1 Nickel 36 41 50.5 Iron bal bal bal (Typical values to guide selection; not a...