1-1 of 1 Search Results for

UNS N10629

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2002) 51 (6): Ni-498.
Published: 01 June 2002
... Copyright ┬ę ASM International┬« 2002 2002 ASM International chemical composition corrosion-resistant alloys elasticity hardness heat treatability joinability machinability Nimofer 6629 physical properties tensile properties workability thermal properties UNS N10629 DOI: 10.31399...