1-2 of 2 Search Results for

UNS N08020, N08825

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2011) 60 (4): SS-1089.
Published: 01 April 2011
...-resistant alloys fracture toughness hardness joinability KUBOTA ALLOY CN-7M physical properties tensile properties UNS N08020, N08825 DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2011, ASM International®. All rights reserved. Data shown are typical, not to be used for specification or final...
Journal Articles
Alloy Digest (2001) 50 (4): Ni-563.
Published: 01 April 2001
... joinability physical properties RA825 tensile properties thermal properties UNS N08825 RA825 (Corrosion Resistant Nickel-Base Alloy) RA825 is a Ni-Fe-Cr-Mo-Cu-Ti alloy with good aqueous corrosion resistance to reducing acids. Applications include the handling of phos- phoric and sulfuric acid...