Alloy Digest (2021) 70 (10): Ni-776.
Published: 01 October 2021
... Copyright © ASM International® 2021 2021 ASM International ATI X-751 chemical composition corrosion-resistant alloys hardness heat treatability joinability machinability physical properties thermal properties workability UNS N07751 ATI X-751 (Nickel-Base Superalloy) Filing Code: Ni-776...
Journal Articles
Alloy Digest (2006) 55 (2): Ni-630.
Published: 01 February 2006
... 7016Titanium-Aluminum physical properties tensile properties workability thermal properties UNS N07751 Chromium 14.0 17.0 Iron 5.0 9.0 Carbon 0.08 max Manganese 1.00 max Silicon 0.50 max Copper 0.50 max Aluminum 0.9 1.50 Titanium 2.00 2.50 Niobium 0.70 1.20 Sulfur 0.010 max Nickel bal...