1-1 of 1 Search Results for

UNS N07626

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1999) 48 (6): Ni-554.
Published: 01 June 1999
... power plant applications oil fields paper industry powder metal products UNS N07626 CRUCIBLE P/M 625M (Heat Treatable Nickel-Base CRA) Crucible P/M 625M is a powder metallurgy (P/M) produced alloy where the composition meets both high-strength and corrosion-resistance re- quirements. P/M 625M is...