Skip Nav Destination
Close Modal
Search Results for
UNS N06950
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-2 of 2 Search Results for
UNS N06950
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (12): Ni-629.
Published: 01 December 2005
... properties workability thermal properties UNS N06950 Chemical Composition, wt (Nominal) Chromium 19.0 21.0 Molybdenum 8.0 10.0 Iron 15.0-20.0 Silicon 1.0 max Carbon 0.02 max Manganese 1.0 max Phosphorus 0.04 max Sulfur 0.015 max Copper 0.50 max Niobium 0.50 max Cobalt 2.50 max Aluminum 0.40 max...
Abstract
View article
PDF
Inconel alloy 050 is an improved corrosion-resistant alloy in tubular form for down hole service. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming. Filing Code: Ni-629. Producer or source: Special Metals Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (2): Ni-423.
Published: 01 February 1993
... hardness HASTELLOY G-50 ALLOY high-temperature alloys physical properties tensile properties tubular products thermal properties UNS N06950 Filing Code: Ni-423 HASTELLOY@ G-50TM ALLOY Nicke FEBRUARY 1993 - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS FYJw2. AkblmJpyg= =ewed P-by: Aby Digrl. k...
Abstract
View article
PDF
HASTELLOY G-50 alloy solves specific needs for applications in sour gas service when strength and corrosion resistance are needed. The alloy is available in tubular products. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high temperature performance, and corrosion resistance. Filing Code: Ni-423. Producer or source: Haynes International Inc.