Alloy Digest (2017) 66 (12): Ni-740.
Published: 01 December 2017
... corrosion-resistant alloys elasticity fracture toughness Nippon Sumitomo Super625 physical properties tensile properties workability high-temperature alloys thermal properties UNS N06852 Nippon Sumitomo Super625 is a nickel alloy with an optimization of compositional elements for thermal...