Alloy Digest (2014) 63 (9): Ni-717.
Published: 01 September 2014
... corrosion-resistant alloys creep properties elasticity Nippon/Sumitomo HR6W physical properties tensile properties workability high-temperature alloys thermal properties UNS N06674 DATA ON WORLDWIDE METALS AND ALLOYS Published by: ASM International Data shown are typical, not to be used for...