1-11 of 11

Search Results for UNS N06625 Grade 2

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2019) 68 (5): Ni-753.
Published: 01 May 2019
... strength high-temperature alloys joinability machinability Nicrofer 6022 hMo oxidation resistance physical properties tensile properties thermal properties UNS N06625 Grade 2 Nicrofer 6022 hMo, a Ni-Cr-Mo-Nb material also called Alloy 625H, is an alloy that combines high-creep strength...
Journal Articles
Alloy Digest (2002) 51 (12): Ni-597.
Published: 01 December 2002
... cladding of the INCO- CLAD tubes is the same as that of conventional alloy 625 tubes and is specified by ASTM B 444, UNS N06625. The grade and composition of the steel substrate are dependent on the steel specified. Some of the common boiler steel grades used for the tube core are ASTM A 210 grade A-1...
Journal Articles
Alloy Digest (2020) 69 (6): Ni-760.
Published: 01 June 2020
... be engaged at all times. Welding VDM 625 can be joined by all conventional welding processes. For welding, VDM 625 should be in the soft or solution annealed condition, and be free from scale, grease, and markings. Comparable Grades VDM Metals ISO EN ASTM VDM 625 UNS N06625 NiCr22Mo9Nb (2.4856) UNS N06625...
Journal Articles
Alloy Digest (2003) 52 (1): Ni-599.
Published: 01 January 2003
... hardness joinability machinability RIMA 625 (62-50) tensile properties weldability UNS N06625 Chemical Composition, wt (Weld metal deposit) Range Typical Carbon 0.05 max 0.015 Manganese 0.50 max 0.02 Silicon 0.50 max 0.1 Sulfur 0.015 max 0.005 Phosphorus 0.015 max 0.005 Chromium 20.0 23.0 22...
Journal Articles
Alloy Digest (2002) 51 (3): Ni-581.
Published: 01 March 2002
... Nimrod 625 and 625KS are Inconel-type consumables with molybdenum and niobium. They are used to join UNS N06625 and Nicrofer 6020hMo of similar composition and also for other lower alloys to ensure the weld has as good or better corrosion resistance as does the base metal. This datasheet provides...
Journal Articles
Alloy Digest (2002) 51 (11): Ni-594.
Published: 01 November 2002
... alloys under cyclic heating and cooling conditions. Specification Equivalents: This alloy is specified as UNS N06626. It can be dual certified since it also meets the requirements of the standard grade from which it was developed (UNS N06625) and which is specified in AMS 5599. AL 625HP is also covered...
Journal Articles
Alloy Digest (2006) 55 (12): Ni-645.
Published: 01 December 2006
... properties UNS N06625 Chemical Composition, wt (Average) Carbon 0.050 Chromium 21.00 Molybdenum 8.50 Cobalt 1.00 max Iron 3.00 max Titanium 0.40 max Aluminum 0.18 Niobium 3.40 Nickel bal Physical Properties: Density, 20 °C (68 °F), kg/m3 (lb/in.3) 8400 (0.303) Thermal conductivity, W/m . K (Btu/(ft . h...
Journal Articles
Alloy Digest (2007) 56 (2): SS-985.
Published: 01 February 2007
... are highly recommended. Carefully grind strike marks and other welding defects; Use run-on and run- off plates and antispatter protection where possible; Dry electrodes according to manufacturer s instructions; An upgraded alloy such as UNS N06625 may be necessary to have the weld corrosion resistance equal...
Journal Articles
Alloy Digest (2004) 53 (9): SS-907.
Published: 01 September 2004
... alloy such as UNS N06625 may be necessary to have the weld corrosion resistance equal to the base metal. Corrosion Resistance: Because of its well-balanced composition consisting of a 18% Ni and high chromium, molybdenum, and nitrogen additions, UR B25 alloy is a typical multipurpose austenitic grade...
Journal Articles
Alloy Digest (2001) 50 (9): SS-829.
Published: 01 September 2001
... Test Results Typical composition, wt% Weight change following Alloy UNS No. Cr Mo Ni 100 test cycles, % AL 409HP S40930 11 57.4 AL 439HP S43035 18 28.9 Type 444 S44400 18 2 +8.1 Type 304 S30400 18 8 47.5 Alloy 625 N06625 21 9 62 +0.1 ...
Journal Articles
Alloy Digest (1993) 42 (12): Ni-443.
Published: 01 December 1993
... thermal properties UNS N06625 Filing Code: Nickel Alloy Ni-443 - DIGEST- DECEMBER 1993 DATA ON WORLD WIDE METALS AND ALLOYS OcapvrisM 1993, Alby LX.qs61. Inc. All rights r66ened PutJirhedby: Alloy Digest Inc 1201-677.9161 Datashorwrar.e~ncftobBusdlor spedcatti m fnal d%@n. ALTEMP= 625 27 Canliild...