Journal Articles
Alloy Digest (2011) 60 (6): Ni-691.
Published: 01 June 2011
... ATI 625HP is a restricted composition of UNS N06625 with exceptional fatigue resistance. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well...
Journal Articles
Alloy Digest (2001) 50 (8): Ni-572.
Published: 01 August 2001
... Sandvik Sanicro 63 was developed specifically for use as outer cladding of composite tubes in service as superheater materials for waste-derived fuel plants. It is a modification of UNS N06625. Typical inner components of the composite tubes are Sandvik 4L7 and Sandvik HT8. This datasheet provides...
Journal Articles
Alloy Digest (2002) 51 (3): Ni-581.
Published: 01 March 2002
... Nimrod 625 and 625KS are Inconel-type consumables with molybdenum and niobium. They are used to join UNS N06625 and Nicrofer 6020hMo of similar composition and also for other lower alloys to ensure the weld has as good or better corrosion resistance as does the base metal. This datasheet provides...
Journal Articles
Alloy Digest (2002) 51 (12): Ni-597.
Published: 01 December 2002
... INCOCLAD625/Steel is a bimetallic clad tube with alloy 625 (UNS N06625) on the outside and with a metallurgical bond holding the alloys together. This datasheet provides information on composition. It also includes information on corrosion resistance as well as forming and joining. Filing Code: Ni...
Journal Articles
Alloy Digest (2003) 52 (1): Ni-599.
Published: 01 January 2003
... hardness joinability machinability RIMA 625 (62-50) tensile properties weldability UNS N06625 Chemical Composition, wt (Weld metal deposit) Range Typical Carbon 0.05 max 0.015 Manganese 0.50 max 0.02 Silicon 0.50 max 0.1 Sulfur 0.015 max 0.005 Phosphorus 0.015 max 0.005 Chromium 20.0 23.0 22...
Journal Articles
Alloy Digest (1999) 48 (7): Ni-555.
Published: 01 July 1999
... International chemical composition corrosion-resistant alloys Crucible P/M N625 microstructure powder metal products tensile properties thermal stability UNS N06625 CRUCIBLE P/M N625 (Powder Metallurgy (P/M) Corrosion-Resistant Nickel Alloy) Crucible P/M N625 is a powder metallurgical nickel-base...
Journal Articles
Alloy Digest (2020) 69 (6): Ni-760.
Published: 01 June 2020
... joinability pressure vessels thermal properties UNS N06625 DOI: 10.31399/asm.ad.ni0760 VDM 625 (Nickel-Chromium-Molybdenum-Niobium Alloy) Filing Code: Ni-760 Nickel :: June 2020 :: :: :: ::Materials Park, Ohio 44073-0002 440.338.5151 Fax 440.338.4634 www.asminternational.org MemberServiceCenter...
Journal Articles
Alloy Digest (2014) 63 (8): Ni-714.
Published: 01 August 2014
...® 2014 2014 ASM International chemical composition corrosion-resistant alloys elasticity heat treatability HPM 625 joinability machinability oxidation resistance physical properties tensile properties workability thermal properties UNS N06625 DATA ON WORLDWIDE METALS AND ALLOYS...
Journal Articles
Alloy Digest (2003) 52 (8): Ni-612.
Published: 01 August 2003
... International chemical composition elasticity fatigue resistance HAYNES ALLOY No. 625SQ heat treatability high-temperature alloys microstructure physical properties superalloys tensile properties thermal properties UNS N06625 Chemical Composition, wt (Nominal) Cobalt 1 max Iron 5 max Chromium...
Journal Articles
Alloy Digest (2002) 51 (11): Ni-594.
Published: 01 November 2002
...-resistant alloys elasticity joinability physical properties tensile properties workability thermal properties UNS N06626 N06625 Chemical Composition, wt Carbon 0.03 max Manganese 0.50 max Phosphorus 0.015 max Sulfur 0.015 max Silicon 0.15 max Chromium 20.0 23.0 Molybdenum 8.0 10.0 Niobium plus...
Journal Articles
Alloy Digest (2019) 68 (5): Ni-753.
Published: 01 May 2019
... strength high-temperature alloys joinability machinability Nicrofer 6022 hMo oxidation resistance physical properties tensile properties thermal properties UNS N06625 Grade 2 Nicrofer 6022 hMo, a Ni-Cr-Mo-Nb material also called Alloy 625H, is an alloy that combines high-creep strength...
Journal Articles
Alloy Digest (2006) 55 (7): Ni-640.
Published: 01 July 2006
... joinability machinability physical properties shear strength tensile properties workability thermal properties UNS N06625 Chemical Composition, wt (Nominal) Carbon 0.10 max Manganese 0.50 max Silicon 0.50 max Chromium 20.00 23.00 Molybdenum 8.00 10.00 Niobium 3.15 4.15 Aluminum 0.40 max Titanium...
Journal Articles
Alloy Digest (2006) 55 (12): Ni-645.
Published: 01 December 2006
... properties UNS N06625 Chemical Composition, wt (Average) Carbon 0.050 Chromium 21.00 Molybdenum 8.50 Cobalt 1.00 max Iron 3.00 max Titanium 0.40 max Aluminum 0.18 Niobium 3.40 Nickel bal Physical Properties: Density, 20 °C (68 °F), kg/m3 (lb/in.3) 8400 (0.303) Thermal conductivity, W/m . K (Btu/(ft . h...
Journal Articles
Alloy Digest (2007) 56 (1): Ni-646.
Published: 01 January 2007
... workability thermal properties UNS N06625 Chemical Composition, wt (Nominal) Chromium 21.0 Molybdenum 9.0 Iron <5.0 Titanium 0.3 Aluminum 0.2 Niobium 3.5 Nickel bal Physical Properties: Melting point, °C (°F) 1290 1350 (2355 2460) Density, kg/m3 (lb/in.3) 8440 (0.305) Resistivity, 20 °C (68 °F), d · m...
Journal Articles
Alloy Digest (1983) 32 (4): Ni-285.
Published: 01 April 1983
...-reactor components oxidation resistance physical properties tensile properties workability UNS N06625 All JESSOP JS625 Flllng Code: Ni-285 Or Nickel Alloy APRIL 1983 DIGEST - DATA ON WORLD WIDE MeTAls AND AUOYS @ Copyright 1980, Engineering Publications. Inc. Ail rights reserved. Published b t MN...
Journal Articles
Alloy Digest (2017) 66 (10): Ni-737.
Published: 01 October 2017
... to intermetallic precipitation during welding. Sanicro 59 is used for joining matching alloys or dissimilar joining to other nickel alloys such as UNS N10276 (2.4819), type UNS N06022 (2.4602), UNS N06625 (2.4856), and N08825 (2.4858). It provides strong, tough, Nb-free weld metal for dissimilar welds in super...
Journal Articles
Alloy Digest (1982) 31 (5): Ni-275.
Published: 01 May 1982
...: Vereingte Deutsche Metallwerke AG Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys elasticity heat treatability joinability machinability NICROFER 6020 HMo oxidation resistance physical properties workability UNS N06625...
Journal Articles
Alloy Digest (1996) 45 (12): Ni-519.
Published: 01 December 1996
... gas turbines applications hardness machinability oxidation resistance physical properties powder metal products pulp equipments UNS N06625 c 3 izszENi~ Y -lJ DATA ON WORLD WIDE METALS AND ALLOYS ANVAL 625 (Ni-Cr-Mo Superalloy Powder) ANVAL 625 is a corrosion- and oxidation-resistant coating...
Journal Articles
Alloy Digest (1992) 41 (8): Ni-409.
Published: 01 August 1992
.... Carlson Inc. Copyright © ASM International® 1996 1996 ASM International CARLSON ALLOY C625 chemical composition corrosion-resistant alloys fatigue properties heat treatability joinability machinability oxidation resistance physical properties tensile properties workability UNS N06625...
Journal Articles
Alloy Digest (2011) 60 (2): Ni-687.
Published: 01 February 2011
.... It is superior to conventional stainless steels such as 316L, however, in seawater applications Alloy 825 does not provide the same levels of resistance as SSC- 6MO(UNS N08367) or Alloy 625(UNS N06625). See Table 5. General Characteristics: Alloy 825 (UNS NO8825) is an austenitic nickel-iron-chromium alloy...