Alloy Digest (1991) 40 (1): Ni-391.
Published: 01 January 1991
... UNS No. N06600 is a nickel-chromium-iron alloy with good resistance to corrosion and heat. It is a solid-solution alloy that can be hardened only by cold working and it has excellent mechanical properties with good workability. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2020) 69 (4): Ni-758.
Published: 01 April 2020
... Special Metals Inconel Alloy 600 (UNS N06600 / Werkstoff Number 2.4816) is a nickel-chromium-iron alloy that is intended for corrosion-resistant and heat-resistant applications. Its versatility has led to its use in a variety of applications involving temperatures from cryogenic to above 1095 °C...
Journal Articles
Alloy Digest (2015) 64 (2): Ni-721.
Published: 01 February 2015
... workability thermal properties UNS N06600 DMV 600/600H are nickel alloys with 15.5 Cr. These stable, fully austenitic solid-solution alloys have higher carbon than alloy 600L (See Alloy Digest Ni-702). Chemical Composition, wt (Typical values, maximum) Carbon 0.025 0.10 Silicon 0.50 Manganese 1.00...
Journal Articles
Alloy Digest (2011) 60 (3): Ni-688.
Published: 01 March 2011
... UNS N06600 DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2011, ASM International®. All rights reserved. Data shown are typical, not to be used for specification or final design. Published by: ASM International, Materials Park, OH 44073-0002, 440-338-5151 MemberServiceCenter@asminternational.org...
Journal Articles
Alloy Digest (2012) 61 (10): Ni-702.
Published: 01 October 2012
... 2012 ASM International chemical composition corrosion-resistant alloys DMV 600L elasticity heat treatability high-temperature alloys joinability physical properties tensile properties workability thermal properties UNS N06600 DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2012, ASM...
Journal Articles
Alloy Digest (2006) 55 (3): Ni-633.
Published: 01 March 2006
... can be readily welded using all the conventional processes. No preweld or postweld treatment is necessary. However, for applications involving a risk of stress-corrosion cracking, a stress-relieving treatment is recommended after welding. UNS N06600 ASTM B 167, B 168 AFNOR NC15Fe...
Journal Articles
Alloy Digest (2012) 61 (6): Ni-697.
Published: 01 June 2012
... International Bohler L312 VMR chemical composition creep properties elasticity fracture toughness heat treatability high-temperature alloys industrial furnaces machinability physical properties tensile properties workability thermal properties UNS N06600 DATA ON WORLDWIDE METALS AND ALLOYS...
Journal Articles
Alloy Digest (1977) 26 (2): Ni-240.
Published: 01 February 1977
... resistance physical properties shear strength tensile properties workability UNS N06600 NlMA660 Filing Code: N i-240 Nickel Alloy FEBRUARY 1977 DIGESTa - DATA ON WORLD WIDE METALS AND ALLOYS Pnblisbod by Engineering ABoys Digest, 1r.1~ Upper Montclair, New Jersey NIMAG 60 (Corrosion and Heat...
Journal Articles
Alloy Digest (1994) 43 (5): Ni-453.
Published: 01 May 1994
... or UNS N06600. NICROBELL B is superior to both of these, and many other commonly used Mineral Insulated cable (MI) sheathing alloys, in the respect that it is complimentary to, and compatible with, the thermoelement conductors. Failure of the thermocouples due to differential coeffi- cient of expansion...
Journal Articles
Alloy Digest (2001) 50 (6): Ni-568.
Published: 01 June 2001
... hardness heat treatability high-temperature alloys joinability machinability NICROFER 7216LC physical properties tensile properties workability thermal properties UNS N06600 Nicrofer 7216 LC is a special low-carbon version of Nicrofer 7216 with carbon at 0.025 wt.% maximum. NICROFER® 7216LC...
Journal Articles
Alloy Digest (1983) 32 (6): Ni-287.
Published: 01 June 1983
... chemical processing applications corrosion-resistant alloys elasticity food processing applications heat resistance heat treatability JESSOP JS600 joinability machinability physical properties tensile properties workability UNS N06600 All JESSOP JS600 Filing Code: Ni-287 Nickel Alloy...
Journal Articles
Alloy Digest (2003) 52 (4): Ni-606.
Published: 01 April 2003
... to weld alloy 600 (UNS N06600), alloy 800 (UNS N08800), alloy DS, Brightray, and other nickel alloys to themselves and to mild or low-alloy steels and stainless steels. Metrode 20.70 Nb is also used for low-tem- perature applications such as in welding 3% or 5% Ni steels used for cryogenic vessels...
Journal Articles
Alloy Digest (1989) 38 (4): Ni-370.
Published: 01 April 1989
... fracture toughness heat treatability joinability machinability oxidation resistance physical properties tensile properties workability UNS N06600 ALLEGHENY LUDLUM AL600 ALLOY Filing Code: Ni-370 Nickel Alloy APRIL 1989 -DIGEST - DATA ON WORLD WIDE METALS AND ALLOYS Publithedby: Aky Digest, Inc...
Journal Articles
Alloy Digest (1995) 44 (7): Ni-483.
Published: 01 July 1995
...-resistant alloys elasticity hardness heat treatability joinability physical properties Sanicro 70 tensile properties thermal properties UNS N06600 - DIGEST& SANDVlK SANICRO 70 ii%t; Ni-483 I 1 DATA ON WORLD WIDE METALS AND ALLOYS JULY 1995 SANDVIK SANICRO 70 PutJirhedby. Abq @ESI. ICC I201.677...
Journal Articles
Alloy Digest (2003) 52 (3): Ni-603.
Published: 01 March 2003
...: Metrode Nimrod AKS and A, as well as Nimax A are Inconel- type consumables similar to the 182, but with lower manganese and with a molybdenum addition. The materials can be used to weld alloy 600 (UNS N06600), alloy 800 (UNS N08800), alloy DS, Brightray, and other nickel alloys to themselves and to mild...
Journal Articles
Alloy Digest (1994) 43 (11): Ni-470.
Published: 01 November 1994
... physical properties tensile properties workability thermal properties UNS N06600 CARLSON ALLOY C600 AND C600 ESR Filing Code: Nickel Alloy Ni-470 - DIGEST- NOVEMBER 1994 DATA ON WORLD WIDE METALS AND ALLOYS eccwqd lsM+Y&?w Ihc.m*- Pt&#BhdW Aby DigaL lnc I201-S77-9161 Effrbdb 27CanfWlSueqOr...
Journal Articles
Alloy Digest (1985) 34 (1): Ni-309.
Published: 01 January 1985
... treatability joinability machinability NICKEL 600 nuclear applications oxidation resistance pharmaceutical applications physical properties tensile properties workability UNS N06600 Nickel Alloy 600 Filing Code: Ni-309 Nickel Alloy JANUARY 1996 - DATA ON WORLD WIDE METALS AND ALLOYS Puhlishrd hv...
Journal Articles
Alloy Digest (1996) 45 (11): Ni-518.
Published: 01 November 1996
... 1996 ASM International chemical composition corrosion-resistant alloys elasticity hardness heat treatability joinability machinability Nicrofer 7216 oxidation resistance physical properties tensile properties workability thermal properties UNS N06600 --m Filing Code: Ni-518...
Journal Articles
Alloy Digest (1997) 46 (1): Ni-520.
Published: 01 January 1997
... workability thermal properties UNS N06600 1 NICROFER@7216 H 1 DATA ON WORLD WIDE METALS AND ALLOYS NICROFER@ 7216 H (Nickel-Chromium-Iron Alloy) Nicrofer 7216 H is a solution-treated nickel-chromium-iron alloy with good resistance to oxidation. carburization. and nitriding; good resistance to stress...