Journal Articles
Alloy Digest (2002) 51 (7): Ni-586.
Published: 01 July 2002
... International® 2002 2002 ASM International chemical composition corrosion-resistant alloys creep properties creep rupture strength elasticity heat treatability high-temperature alloys joinability physical properties RA602CA tensile properties workability thermal properties UNS N06025...
Journal Articles
Alloy Digest (1997) 46 (4): Ni-523.
Published: 01 April 1997
... 1997 1997 ASM International chemical composition corrosion-resistant alloys creep properties elasticity fatigue properties heat treatability joinability machinability microstructure Nicrofer 6025 HT oxidation resistance physical properties workability thermal properties UNS N06025...