... treatability joinability machinability military applications motorsport applications physical properties shear strength tensile properties thermal properties UNS M18410 ELEKTRON WE54 (Heat Treatable Magnesium Casting Alloy) ElektronWE54 is fully heat treatable for use to 300 °C (570 °F) and is free...