Alloy Digest (2018) 67 (6): Mg-85.
Published: 01 June 2018
... physical properties shear strength tensile properties thermal properties UNS M18010 Magnesium K1A is the casting alloy with the highest vibration-damping index. Chemical Composition, wt.% (Nominal) Designation K1A UNS M18010 Zirconium 0.40 1.0 Total impurities, max 0.3 Magnesium bal Physical...