Alloy Digest (2017) 66 (8): Fe-167.
Published: 01 August 2017
... purification of the metal. The optimum heat treatment is 4 hours at 1150 °C (2102 °F) in pure dry hydrogen. Mechanical Properties: See Table 2 for mechanical properties of strip. Specification Equivalents: ASTM A753, A596 DIN 17405 EN 10252 IEC 404 JIS C 2531 LMSA F112 UNS K94840 Alloy Type 2 General...
Journal Articles
Alloy Digest (2013) 62 (6): Fe-160.
Published: 01 June 2013
... tensile properties workability UNS K94800, K94840 DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2013, ASM International®. All rights reserved. Data shown are typical, not to be used for specification or final design. Published by: ASM International, Materials Park, OH 44073-0002, 440-338-5151...