Alloy Digest (2006) 55 (3): Fe-138.
Published: 01 March 2006
... joinability physical properties tensile properties workability thermal properties UNS K93601, K94100, N14052 (Nominal) Ni36 Ni42 Ni52 Carbon 0.01 Manganese 0.30 0.40 0.30 Silicon 0.20 0.1 Nickel 36 41 50.5 Iron bal bal bal (Typical values to guide selection...