Alloy Digest (1989) 38 (12): SA-443.
Published: 01 December 1989
... PYROWEAR ALLOY 53 tensile properties workability UNS K71040 DECEMBER 1989 -DIGEST - DATA ON WORLD WIDE METALS AND ALLOYS Ccpy@hl MS, A&y ajlal. k All tights mssrvsd. Pubfish& by: AUoy Digal. Inc. /x)1-677-9161 Dala*amlpkd,nollokudla 27 Canfisld Slmt. Orange. N.J. 07060 I U.S.A. sflmadm w hal design...