Skip Nav Destination
Close Modal
Search Results for
UNS K20747
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Subjects
Journal
Article Type
Date
Availability
1-1 of 1
Search Results for UNS K20747
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1990) 39 (4): SA-446.
Published: 01 April 1990
... Code: SA-446. Producer or source: Bethlehem Steel Corporation. Producer or Source: Bethlehem Steel Corporation Copyright © ASM International® 1996 1996 ASM International ASTM A710 chemical composition fracture toughness heat treatability joinability tensile properties UNS K20747...
Abstract
View articletitled, ASTM A710: Low Carbon, Precipitation Hardening High-Strength Alloy Steel
View
PDF
for article titled, ASTM A710: Low Carbon, Precipitation Hardening High-Strength Alloy Steel
ASTM A710 is a low-carbon, precipitation hardening high-strength alloy steel plate. It is well suited to critical applications. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on heat treating and joining. Filing Code: SA-446. Producer or source: Bethlehem Steel Corporation.