Alloy Digest (1982) 31 (6): SS-410.
Published: 01 June 1982
... machinability petrochemical industry physical properties power industry tensile properties UNS J94213 ACI Type HN Filing Code: ss-410 Stainless Steel JUNE 1982 - DATA ON WORLD WIDE METALS AND ALLOYS @ Copyright 1980. Engineering Publications, Inc. Ail rights reserved. MN : 002-614X Publidml by En@neming...