Alloy Digest (1988) 37 (6): SA-430.
Published: 01 June 1988
... UNS No. H47180 is a low-carbon nickel-chromium-molybdenum carburizing steel recommended for applications requiring a strong, tough core combined with a highly wear-resistant carburized case. It has fairly high hardenability and can be used without carburizing. This datasheet provides information...