Alloy Digest (1980) 29 (12): SA-379.
Published: 01 December 1980
... joinability machinability physical properties shafts tensile properties workability UNS G86270 H86270 AM 8627 Filing Code: SA-379 Steel-Alloy DECEMBER 1980 - DATA ON WORLD WIDE METALS AND ALLOYS Q Copyright 1980. Engineering Publications. Inc. A41 rights reserved. ISSN: 002-614X Publid...