Alloy Digest (1990) 39 (10): SA-452.
Published: 01 October 1990
... UNS G50460 is an alloy steel of fairly low hardenability. It is used in a number of machinery and engineering applications where its relatively low hardenability and moderate strength are satisfactory. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1985) 34 (3): SA-408.
Published: 01 March 1985
...(5OB46). SAE: J404(50846). J412(50B46) and J770(5OB46). General Characteristics: UNS No. G50461 (AISI 508461 IS a boron-treated low-chromium steel with a much higher hardenability than the corresponding boron-free steel UNS No. G50460 (AISI 5046). The higher hardenability of UNS No. G50461 results from...