Alloy Digest (2004) 53 (2): SA-436.
Published: 01 February 2004
... workability thermal properties UNS G11190, G11440 Chemical Composition, wt C1119 C1144 Carbon 0.17 0.23 0.40 0.50 Manganese 1.00 1.30 1.00 1.30 Phosphorus 0.04 max 0.03 max Sulfur 0.20 0.33 0.20 0.33 Silicon 0.15 max 0.10 max Iron bal bal Physical Properties: (For C1119 only) Specific gravity 7.82...