Alloy Digest (1986) 35 (8): CS-112.
Published: 01 August 1986
... UNS No. G10860 is a high-carbon oil or water-hardening steel of low hardenability. It develops high surface hardness on quenching rapidly and tempering lightly and it has good resistance to wear. It is used for tools, springs, music wire, machinery parts and many other applications. This datasheet...