Skip Nav Destination
Close Modal
Search Results for
UNS C95200
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-2 of 2 Search Results for
UNS C95200
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1977) 26 (2): Cu-326.
Published: 01 February 1977
... properties tensile properties wear resistance welding jaws UNS C95200 Filing Code: Cu-326 v Copper Alloy No. 952 Copper Alloy FEBRUARY 1977 DIGESTa - DATA ON WORLD WIDE METALS AND ALLOYS Psblisbrd by Engineering Alloys Digest, Inc. Upper Montclair. New Jersey Copper Alloy No. 952 (Cast Aluminum Bronze...
Abstract
View article
PDF
Copper Alloy No. 952 is a cast alloy offering high strength, high hardness, excellent resistance to corrosion and good resistance to fatigue and wear. It is well suited for temperatures up to 750 F for such applications as gears, welding jaws and electrical hardware. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-326. Producer or source: Copper alloy foundries.
Journal Articles
Alloy Digest (1979) 28 (6): Cu-374.
Published: 01 June 1979
... hardness heat treatability joinability machinability marine hardware physical properties pickling equipment propellers shear strength tensile properties wear resistance UNS C95200 Filing Code: cu-374 I Copper Alloy Or JUNE 1979 BIGlST - DATA ON WORLD WIDE METALS AND ALLOYS - p-by yg&vh% h...
Abstract
View article
PDF
AMPCO A-1 is a cast copper-base alloy well suited for use up to 750 F. It is characterized by fairly high hardness and strength, good resistance to fatigue and wear, and excellent corrosion resistance. Among its many applications are acid-resisting pumps, pickling equipment, gears, marine hardware and propellers. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-374. Producer or source: Ampco Metal Inc..