Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (9): Cu-528.
Published: 01 September 1987
... alloys elasticity fatigue properties fracture toughness hardness heat treatability joinability locomotive wearing parts machinability physical properties shear strength tensile properties UNS C94500 Copper Alloy No. C94500 Filing Code: Cu-528 Copper Alloy SEPTEMBER 1887 - DATA ON WORLD...