Skip Nav Destination
Close Modal
Search Results for
UNS C91000
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
UNS C91000
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (12): Cu-531.
Published: 01 December 1987
... physical properties piston rings tensile properties UNS C91000 Copper Alloy No. C91000 Filing Code: Cu-531 Copper Alloy - DATA ON WORLD WIDE METALS AND ALLOYS DECEMBER 1987 Fublhed by: Alloy D&s, lnc 27 Car&Id SUUI Omn~ New Jersey 07050 (201) 677-9161 Copper Alloy No. C91000 (Cast Copper-Tin Alloy...
Abstract
View article
PDF
Copper Alloy No. C91000 is a cast copper-tin alloy which also is known by names formerly used (but not recommended): 197, Tin Bronze and 85-14-0-1. It is a medium-strength alloy and has a good combination of strength, ductility and resistance to corrosion. Its uses include piston rings and bearings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-531. Producer or source: Copper alloy foundries.