Alloy Digest (1982) 31 (2): Cu-432.
Published: 01 February 1982
... properties valves UNS C90500 Filing Code: Cud2 COPPER ALLOY No. C90500 copperAl oy FEBRUARY 1982 B DATA ON WORLD WIDE METALS AND AU.oYs -bu @ Copyright 1980. Engiwring Publiwtions. Inc. Ail righk reswved. ISSN:OO2-614X UpperMcdchir,NewJemey Copper Alloy No. C90500 (Cast Tin Bronze) Copper Alloy...
Journal Articles
Alloy Digest (1978) 27 (8): Cu-358.
Published: 01 August 1978