Alloy Digest (2019) 68 (7): Cu-891.
Published: 01 July 2019
... hardness interchangeable physical properties tensile properties thermal properties UNS C89833 Concast C89833 is a lead-free casting alloy that can be interchangeable with C836. It is classified as a bismuth tin bronze. See Alloy Digest Cu-611 and Cu-317. Chemical Composition, wt.% (Nominal, maximum...
Journal Articles
Alloy Digest (1997) 46 (4): Cu-612.
Published: 01 April 1997
... composition compressive strength corrosion-resistant alloys elasticity Federalloy I-836 fracture toughness hardness joinability machinability physical properties tensile properties thermal properties UNS C89833 DATA ON WORLD WIDE METALS AND ALLOYS FEDERALLOP l-836 (Machinable Lead-Free Bronze...