Alloy Digest (1979) 28 (3): Cu-369.
Published: 01 March 1979
... hardware physical properties propellers tensile strength UNS C86500 AMPCOLOY 62 Filing Code: h-369 Copper Alloy MARCH 1979 Emmu OfGIsT - DATA ON WORLD WIDE METALS AND ALLOYS - -bu AMPCOLOY* 62 (Low-Strength Cast Manganese Bronze) AMPCOLOY 62 is a cast copper-base alloy known as low-tensile manganese...
Journal Articles
Alloy Digest (1977) 26 (11): Cu-344.
Published: 01 November 1977
... castability chemical composition Copper alloy no. 865 corrosion-resistant alloys ductility elasticity gears hardness heat treatability joinability machinability marine hardware physical properties propellers tensile strength UNS C86500 Copper Alloy No. 865 Filing Code: cu-344 Copper Alloy...