Skip Nav Destination
Close Modal
Search Results for
UNS C86200
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-2 of 2
Search Results for UNS C86200
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
AMPCOLOY 64: Cast Medium Strength Manganese Bronze
Available to Purchase
Alloy Digest (1980) 29 (6): Cu-396.
Published: 01 June 1980
... machinability marine hardware physical properties tensile strength UNS C86200 I Filing Code: Cu-396 @lr AMPCOLOY 64 Copper Alloy JUNE 1990 - DATA ON WORLD WIDE MEMLS AND ALLOYS @ Copyright 1980. Engineering Publications. Inc. WI rights reserved. Pubkhed by EIlghmhg Moys Digest, Inc Post office Box 823...
Abstract
View articletitled, AMPCOLOY 64: Cast Medium Strength Manganese Bronze
View
PDF
for article titled, AMPCOLOY 64: Cast Medium Strength Manganese Bronze
AMPCOLOY 64 is a casting alloy that is frequently classified as a high-strength yellow brass; its typical tensile strength is 95,000 psi in the as-cast condition. This alloy has an excellent combination of strength, ductility and resistance to corrosion. Its numerous applications include propellers, bearings, gears and marine hardware. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-396. Producer or source: Ampco Metal Inc..
Journal Articles
COPPER ALLOY No. 862: Cast Medium Tensile Manganese Bronze
Available to Purchase
Alloy Digest (1979) 28 (1): Cu-365.
Published: 01 January 1979
... Copper alloy no. 862 corrosion-resistant alloys ductility elasticity fracture toughness heat treatability joinability machinability marine hardware physical properties tensile strength valve stems UNS C86200 I Filing Code: cu-365 07 Copper Alloy No. 862 Copper Alloy JANUARY 1979 pnemsTB...
Abstract
View articletitled, COPPER ALLOY No. 862: Cast Medium Tensile Manganese Bronze
View
PDF
for article titled, COPPER ALLOY No. 862: Cast Medium Tensile Manganese Bronze
Copper Alloy No. 862 is a copper-zinc-aluminum-manganese-iron alloy; aluminum is the principal strengthening element. It is classified as a high-strength yellow brass; its typical tensile strength is 95,000 psi. It has an excellent combination of strength and ductility along with good resistance to corrosion. Its numerous applications include cams, valve stems and marine hardware. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-365. Producer or source: Copper alloy foundries.