Alloy Digest (1983) 32 (4): Cu-457.
Published: 01 April 1983
... no. C84800 corrosion-resistant alloys creep properties ductility elasticity faucets hardness heat treatability joinability machinability physical properties plumbing components tensile properties UNS C84800 Copper Alloy No. (34800 Filing Code: cu-457 Copper Alloy APRIL 1983 - DATA ON WORLD...