Alloy Digest (1978) 27 (3): Cu-349.
Published: 01 March 1978
... machinability physical properties plumbing goods tensile properties valves UNS C84400 Copper Alloy No. 844 Filing Code: cu-349 Copper Alloy MARCH 1978 - DATA ON WORLD WIDE METALS AND ALLOYS palbhhdbu Copper Alloy No. 844 (Cest Leaded Semi-Red Brass) Copper Alloy No. 844 is a free-cutting copper-tin-lead...
Journal Articles
Alloy Digest (1996) 45 (6): Cu-605.
Published: 01 June 1996
.... Traditional lead plumbing alloys are so highly machinable that cutting fluids are often omitted. Some machines may experience slightly higher tool wear with SeBiLOY compared with either C83600 or C84400 (See A&J Digesr G-31 7 and G-319). The reasons for this effect are not yet fully understood, however...
Journal Articles
Alloy Digest (1996) 45 (7): Cu-606.
Published: 01 July 1996
... may experience slightly higher tool wear with SeBiLOY compared with either C83600 or C84400 (See Alloy Digesr CL317 and Cu-349). The reasons for this effect are not yet fully understood, however, and it seems to vary with type of tooling and machining operation. Measurements show that machined surface...
Journal Articles
Alloy Digest (2001) 50 (3): Cu-662.
Published: 01 March 2001
..., typical 255 37 117 17 30 60 C84400, typical 241 35 97 14 28 55 EnviroBrass I, typical 209 30 136 20 12 71 EnviroBrass I, min 185 27 119 17 8 66 EnviroBrass II, typical 215 31 145 21 10 73 EnviroBrass II, min 176 21 121 18 6 68 C85800, typical 332 48 192 28 90 60 EnviroBrass III, typical 332 48 200 29 8 63...
Journal Articles
Alloy Digest (1997) 46 (4): Cu-612.
Published: 01 April 1997
... during the casting of its alloys. This feature helps highlight the details in a mold. Except for a machining adjustment, the properties of Federalloy compare favorably to alloys UNS C83600 and C84400. This in- cludes mechanical strength, pressure tighmess. corrosion resis- tance. and polishing, buffiig...
Journal Articles
Alloy Digest (1997) 46 (6): Cu-614.
Published: 01 June 1997
... and C84400. This includes mechanical strength. pressure tightness, corrosion resis- tance. and polishing. buffing, and plating. The above-noted prop- erties are all important to the faucet manufacturing industry. With respect to corrosion in water, the leachate rate for lead and bismuth in drinking water...