Skip Nav Destination
Close Modal
Search Results for
UNS C82510
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
UNS C82510
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1992) 41 (8): Cu-575.
Published: 01 August 1992
... machinability physical properties tensile properties UNS C82510 BRUSH CASTING ALLOY 21 C EY QJ-SX - DIGEST- AUGUST 1992 DATA ON WORLD WIDE METALS AND ALLOYS g$4$wt -wp- P-by: AbyDQ%l.ln~1201-677-6161 t?pBcMwolr&~ 27CaniiiSmel.OmqaNJ.070501U.SA BRUSH CASTING ALLOY 21C (High Strength Beryllium Copper Alloy...
Abstract
View article
PDF
BRUSH CASTING ALLOY 21C is a beryllium copper alloy of high strength with cobalt as the second alloying element (1.0 to 2.0% Co). Use is in age-hardened temper. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on casting, heat treating, and machining. Filing Code: Cu-575. Producer or source: Brush Wellman Inc..