Alloy Digest (2019) 68 (10): Cu-897.
Published: 01 October 2019
... or source: Olin Brass and Somers Thin Strip. Producer or Source: Olin Brass and Somers Thin Strip Copyright ┬ę ASM International┬« 2019 2019 ASM International chemical composition OLIN BRASS C75200 physical properties tensile properties workability thermal properties UNS C75200 Olin...