1-7 of 7 Search Results for

UNS C72900

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (9): Cu-588.
Published: 01 September 1993
... properties tensile properties workability thermal properties UNS C72900 Filing Code: Cu-588 COPPER ALLOY NO. C72900 CopperA oy SEPTEMBER 1993 - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS eyright 1993, Alby D&st. Inc. Ail rights resewed. Pub/M&by: Alloy Digest. Inc. / 201-677-9161 maJhownamI...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (10): Cu-802.
Published: 01 October 2011
... alloys elasticity fracture toughness hardness Pfinodal physical properties tensile properties workability thermal properties UNS C72900 DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2011, ASM International®. All rights reserved. Data shown are typical, not to be used for specification...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2014) 63 (6): Cu-832.
Published: 01 June 2014
... dimensional stability elastic strength elasticity hardness physical properties tensile properties workability UNS C72900 DATA ON WORLDWIDE METALS AND ALLOYS Published by: ASM International Data shown are typical, not to be used for specification or final design. Materials Park, OH 44073-0002, 440...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1983) 32 (11): Cu-467.
Published: 01 November 1983
... International chemical composition corrosion-resistant alloys elasticity electrical connectors heat treatability joinability machinability PFINODAL C72900 physical properties powder metal products springs switches tensile properties workability wrought copper alloys UNS C72900 All...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1999) 48 (5): Cu-635.
Published: 01 May 1999
... 0.11Mg-0.06P-0.05Ag 85 C19700 0.6Fe-0.2P-0.05Mg 77 Olin alloy 186 0.5Fe (or Co)-0.3Cr-0.2Ti-0.2Zr 70 C17410 0.5Co-0.3Be 45 C70250 3.0Ni-0.65 Si-0.15 Mg 40 C17200 1.9Be-0.4Co 17 C72900 15Ni-8Sn 7 N03360 97.5Ni-2.0Be-0.5Ti 5 Table 2 Formability Bending of Olin Alloy 186 in Longitudinal (Parallel to Rolling...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2001) 50 (7): Cu-670.
Published: 01 July 2001
... AT 120 827 120 7 32 Table 2 Mechanical Properties of ToughMet 3 Compared to Other Bearing Alloys Yield strength Tensile strength Elongation, Modulus of elasticity Fatigue strength, 108 cycles Material UNS No. Chemical composition, % MPa ksi MPa ksi % Hardness GPa 106 psi MPa ksi ToughMet 3 C96900, C72900...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1994) 43 (6): Cu-598.
Published: 01 June 1994
... is a powder metallurgy produced age-hardenable alloy with less alloy content than C72900 (See Alloy Digest Cu-588). This is particularly advantageous where high electrical conductivity, low work hardening rate, low recrystallization temperature and fine grain size are important. As contacts in connectors...