Alloy Digest (1986) 35 (4): Cu-503.
Published: 01 April 1986
... UNS C72800 Copper Alloy No. C72800 Filing Code: Cu-503 Copper Alloy Revised APRIL 1986 NOVEMBER 1985 Puh/i.dled hr Alloy Digest. Inc. 27 Cantield Street Orange. New Jersey 07050 (201) 7hl-1090 Copper Alloy No. C72800 (High-Strength Corrosion-Resistant Copper-Base Alloy) Copper Alloy No. C72800...