1-7 of 7 Search Results for

UNS C71500

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2006) 55 (6): Cu-744.
Published: 01 June 2006
... ASM International® 2006 2006 ASM International chemical composition corrosion-resistant alloys elasticity HIDURON 107 joinability machinability physical properties seawater applications shear strength tensile properties workability thermal properties UNS C71500 Chemical...
Journal Articles
Alloy Digest (2012) 61 (8): Cu-810.
Published: 01 August 2012
... ELECTRALLOY EC70600 heat treatability joinability machinability physical properties tensile properties workability thermal properties UNS C71500 DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2012, ASM International®. All rights reserved. Data shown are typical, not to be used for specification...
Journal Articles
Alloy Digest (2012) 61 (7): Cu-809.
Published: 01 July 2012
... ELECTRALLOY EC71500 heat treatability joinability machinability physical properties tensile properties workability thermal properties UNS C71500 DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2012, ASM International®. All rights reserved. Data shown are typical, not to be used for specification...
Journal Articles
Alloy Digest (2002) 51 (10): Cu-691.
Published: 01 October 2002
... treatability joinability machinability physical properties tensile properties weldability workability thermal properties UNS C71500 Chemical Composition, wt (Nominal) Carbon 0.05 max Zinc 0.50 max Sulfur 0.02 max Phosphorus 0.02 max Lead 0.02 max Manganese 1.00 max Nickel 29.0 33.0 Iron 0.40 1.0...
Journal Articles
Alloy Digest (1978) 27 (12): Cu-363.
Published: 01 December 1978
... International AMPCOLOY 522 chemical composition corrosion-resistant alloys ductility elasticity hardness heat treatability joinability machinability physical properties tensile properties workability wrought copper alloys UNS C71500 - nATA fiN WftDI n UlllSC METALS AND ALI AMPCOLOY 522...
Journal Articles
Alloy Digest (1988) 37 (1): Cu-534.
Published: 01 January 1988
.... Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys elasticity hardness heat treatability joinability machinability MONEL ALLOY 450 physical properties tensile properties weldability workability UNS C71500 MONEL ALLOY 450 Filing...
Journal Articles
Alloy Digest (2013) 62 (2): Cu-815.
Published: 01 February 2013
... Brass Company as an answer to the need for metal less costly than the richer copper nickel alloys, but still offering much of the properties characteristic of this alloy family. C70600 thus offers, to a good degree, the properties inherent in Cupro Nickel 70/30 C71500, but with its reduced nickel...