Alloy Digest (2010) 59 (1): Cu-778.
Published: 01 January 2010
... corrosion-resistant alloys Eco Brass hardness machinability physical properties tensile properties workability UNS C69300 and C87850 DATA ON WORLDWIDE METALS AND ALLOYS Copyright ┬ę 2010, ASM International┬«. All rights reserved. Data shown are typical, not to be used for specification or final...