Alloy Digest (2011) 60 (8): Cu-801.
Published: 01 August 2011
... elasticity hardness heat treatability joinability physical properties tensile strength WIELAND-FX9 workability thermal properties UNS C66950 DATA ON WORLDWIDE METALS AND ALLOYS Copyright ┬ę 2011, ASM International┬«. All rights reserved. Data shown are typical, not to be used for specification...