... composition elasticity hardness heat treatability joinability machinability physical properties pole line hardware screws tensile properties workability thermal properties UNS C65100 ANSONIA ALLOY C65100 (Low-Silicon Bronze Alloy) Ansonia alloy C65100 is often called low silicon bronze and is...