1-1 of 1 Search Results for

UNS C64210

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1984) 33 (2): Cu-471.
Published: 01 February 1984
... composition corrosion-resistant alloys ductility elasticity hardness heat treatability joinability machinability marine bushings MUELLER ALLOY 6421 nuts physical properties tensile properties workability UNS C64210 1 MUELLER Alloy 6421 Filing Code: Cu-471 Or Copper Alloy FEBRUARY 1994 BfGfsT...