Alloy Digest (1985) 34 (2): Cu-492.
Published: 01 February 1985
... alloys ductility elasticity fatigue properties hardness heat treatability joinability machinability physical properties shear strength tensile properties welding rod workability UNS C61800 - mer Allov No. C618OOI Filing Code: Cu-492 Copper Alloy 1 FEBRUARY 1985 - DATA ON WORLD WIDE...