Skip Nav Destination
Close Modal
Search Results for
UNS C52400
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-3 of 3
Search Results for UNS C52400
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (2018) 67 (10): cu-880.
Published: 01 October 2018
... Alloy Cu-PHC (UNS C52400) is an oxygen-free extra low-phosphorus alloy. Typical uses include electrical devices, switching elements, connectors, and terminals. This datasheet provides information on composition, physical properties, and bend strength. It also includes information on corrosion...
Abstract
View articletitled, KEMPER Cu-PHC: Low-Phosphorus Copper Alloy
View
PDF
for article titled, KEMPER Cu-PHC: Low-Phosphorus Copper Alloy
Alloy Cu-PHC (UNS C52400) is an oxygen-free extra low-phosphorus alloy. Typical uses include electrical devices, switching elements, connectors, and terminals. This datasheet provides information on composition, physical properties, and bend strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-880. Producer or source: Gebr. Kemper GmbH + Company KG Metallwerke.
Journal Articles
Alloy Digest (2018) 67 (8): Cu-877.
Published: 01 August 2018
... International bend strength chemical composition corrosion-resistant alloys electrical conductivity hardness joinability KEMPER CuSn10 physical properties tensile properties thermal conductivity wear resistance workability UNS C52400 Alloy CuSn10 is a high-performance copper alloy. Chemical...
Abstract
View articletitled, KEMPER CuSn10: Copper/Tin Sn Alloy
View
PDF
for article titled, KEMPER CuSn10: Copper/Tin Sn Alloy
Alloy CuSn10 is a high-performance copper alloy. The alloy is characterized by good electrical and thermal conductivity and very good resistance to stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength. It also includes information on corrosion and wear resistance as well as forming and joining. Filing Code: Cu-877. Producer or source: Gebr. Kemper GmbH + Company KG Metallwerke.
Journal Articles
Alloy Digest (1999) 48 (10): Cu-640.
Published: 01 October 1999
... Comparison of Tensile Strength between Phosphor Bronzes and Improved Phosphor Bronzes Tensile strength, MPa (ksi) Temper C51100 WRM 5118 C51000 WRM 5108 C52100 WRM 5218 C52400 WRM 5248 1 2 hard (H02) 390 483 (55 70) 573 676 (83 98) 400 504 (58 73) 600 704 (87 102) 476 580 (69 84) 656 759 (95 110) 524 628 (76...
Abstract
View articletitled, WRM ALLOY 5248: Phosphor Bronze Alloy
View
PDF
for article titled, WRM ALLOY 5248: Phosphor Bronze Alloy
WRM alloy 5248 is a phosphor bronze alloy with higher strength and better stress relaxation resistance than 10% tin alloys. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend strength. Filing Code: CU-640. Producer or source: Waterbury Rolling Mills Inc.