Alloy Digest (2000) 49 (4): Cu-618.
Published: 01 April 2000
... composition physical properties springs tensile properties workability WRM ALLOY 5218 thermal properties UNS C52180 WRM ALLOY 5218 (Modified Phosphor Bronze) WRM Alloy 5218 is a modified phosphor bronze with very good relaxation characteristics and with higher strength compared to standard phosphor...