Alloy Digest (2003) 52 (1): Cu-696.
Published: 01 January 2003
... Wieland-B18 is a phosphor bronze with a composition that allows usage in slightly more severe service conditions than alloy B16 (UNS C52100). A common application is in slide bearings and slideways. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (2018) 67 (7): Cu-875.
Published: 01 July 2018
... Alloy CuSn8 (UNS C52100) is a high-performance copper alloy with 8% tin. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength. It also includes information on wear resistance as well as forming and joining. Filing Code: Cu-875...
Journal Articles
Alloy Digest (2012) 61 (11): Cu-814.
Published: 01 November 2012
... International bend strength chemical composition corrosion-resistant alloys elasticity fatigue properties heat treatability joinability machinability physical properties tensile properties Wieland-B18 Supralloy workability thermal properties UNS C52100 DATA ON WORLDWIDE METALS AND ALLOYS...
Journal Articles
Alloy Digest (2021) 70 (6): Cu-82.
Published: 01 June 2021
... 2021 2021 ASM International chemical composition corrosion resistance elasticity forming hardness heat treating machining physical properties thermal properties Wiel B09/B10 UNS C52100 WIELAND B09/B10 (Cu-8Sn-0.2P Alloy) Filing Code: Cu-82 Copper :: June 2021 Materials Park, Ohio...
Journal Articles
Alloy Digest (2000) 49 (1): Cu-644.
Published: 01 January 2000
.... Specification Equivalents: UNS C42600 General Characteristics: WRM alloy 4260 is a modified copper-zinc-tin alloy with strength and formability similar to C52100, nearly double the electrical conductivity, and improved stress relaxation. This composition provides opportunities for cost reductions via...
Journal Articles
Alloy Digest (2017) 66 (3): Cu-858.
Published: 01 March 2017
... physical properties tensile properties workability thermal properties UNS C19040 Kobelco Alloy CAC 5 has higher stress-relaxation strength. The alloy is nominally Cu-0.8Ni-1.2Sn-0.07P. CAC 5 has the good strength of C52100 and C26000. Chemical Composition, wt (Nominal) Nickel 0.8 Tin 1.2 Phosphorus...
Journal Articles
Alloy Digest (1978) 27 (4): Cu-351.
Published: 01 April 1978
... COPPER ALLOYS AT VARIOUS TEMPERS Property and Temper ChSe UNS UNS UNS UNS 69000 C68800 C52100 C76200 c17500* Conductivity, % IACS 18 18 Tensile Strength, psi Annealed 80000 82000 Quarter hard 94000 94000 Half hard 104000 104000 Hard 113000 113000 Extra hard 120000 120000 Spring 128000 128000 Extra spring...
Journal Articles
Alloy Digest (2000) 49 (4): Cu-618.
Published: 01 April 2000
..., Inc. Waterbury, CT 06708 (800) 243-3002 (203) 754-0151 (203) 754-1061 (fax) ISSN: 002-614X Cu-618B Table 4 Comparison of Tensile Strength between Phosphor Bronzes and Improved Phosphor Bronzes Tensile strength C51100 WRM 5118 C51000 WRM 5108 C52100 WRM 5218 Temper MPa ksi MPa ksi MPa ksi MPa ksi MPa...
Journal Articles
Alloy Digest (1999) 48 (10): Cu-640.
Published: 01 October 1999
... Comparison of Tensile Strength between Phosphor Bronzes and Improved Phosphor Bronzes Tensile strength, MPa (ksi) Temper C51100 WRM 5118 C51000 WRM 5108 C52100 WRM 5218 C52400 WRM 5248 1 2 hard (H02) 390 483 (55 70) 573 676 (83 98) 400 504 (58 73) 600 704 (87 102) 476 580 (69 84) 656 759 (95 110) 524 628 (76...
Journal Articles
Alloy Digest (1986) 35 (5): Cu-509.
Published: 01 May 1986
...% offset yield strength). c51000* 5 Sn 0.2 P I07 9x <8 97 I5 I.3 6.5 -I9 c52100* ChXXOO* X Sn 22.7 Zn 3.4 .4I. 0.4 co I 20 I20 IO5 II7 <5 2 max. I00 99 I3 IX I.1 N .4 1.7 6.5 N .4 8 46 appros 25 approx 55 c72500* 9.5 Ni 2.3 Sn 90- IO5 XX-IO2 I max. x7-95 9 Safe Handling: Beryllium-containing alloys. like...