Journal Articles
Alloy Digest (2018) 67 (4): Cu-870.
Published: 01 April 2018
... International® 2018 2018 ASM International bend strength chemical composition corrosion-resistant alloys formability hardness joinability KEMPER CuSn4 machinability physical properties tensile properties workability thermal properties UNS C51100 Alloy CuSn4 is a high-performance copper...
Journal Articles
Alloy Digest (2002) 51 (8): Cu-686.
Published: 01 August 2002
... workability thermal properties UNS C51100 Chemical Composition, wt Tin 4 Copper bal Physical Properties: Density, kg/m3 (lb/in.3 ) 8850 (0.320) Coefficient of linear thermal 18.0 (10.0) expansion, 10 6/K (10 6/°F) Electrical conductivity, 106 S/m 10 ( 18) (%IACS) Thermal conductivity, 100 (58) W/m K...
Journal Articles
Alloy Digest (2010) 59 (5): Cu-782.
Published: 01 May 2010
... LUVATA C511 machinability physical properties tensile properties workability thermal properties UNS C51100 DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2010, ASM International®. All rights reserved. Data shown are typical, not to be used for specification or final design. Published by: ASM...
Journal Articles
Alloy Digest (2012) 61 (7): Cu-808.
Published: 01 July 2012
... corrosion-resistant alloys elasticity heat treatability joinability physical properties tensile properties Wieland-B14 Supralloy workability thermal properties UNS C51100 DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2012, ASM International®. All rights reserved. Data shown are typical...
Journal Articles
Alloy Digest (1981) 30 (2): Cu-412.
Published: 01 February 1981
... ductility elasticity fasteners hardness heat treatability joinability machinability physical properties springs tensile properties textile machinery workability wrought bronze UNS C51100 Copper Alloy No. C51100 Filing Code: cu-412 Copper Alloy FEBRUARY 1981 - DATA ON WORLD WIDE METALS...
Journal Articles
Alloy Digest (2000) 49 (1): Cu-644.
Published: 01 January 2000
... Yield strength Alloy Temper Conductivity, %IACS MPa ksi MPa ksi WRM 4112 (C41120) 1 2 hard (H02) 40 414 517 60 75 379 483 55 70 C51100 1 2 hard (H02) 20 379 483 55 70 290 483 42 70 WRM 4222 (C42220) 1 2 hard (H02) 35 441 545 64 79 400 503 58 73 C51000 1 2 hard (H02) 15 400 503 58 73 324 469 47 68 WRM...
Journal Articles
Alloy Digest (1999) 48 (10): Cu-636.
Published: 01 October 1999
... Strength Alloy C51100 WRM 5118 Temper MPa ksi MPa ksi 1 2 hard (H02) 379 483 55 70 572 676 83 98 Hard (H04) 496 600 72 87 669 772 97 112 Extra hard (H06) 579 683 84 99 703 807 102 117 Spring (H08) 627 724 91 105 724 827 105 120 Extra spring (H10) 662 752 96 109 758 862 110 125 DOI: 10.31399/asm.ad.cu0636...
Journal Articles
Alloy Digest (2000) 49 (4): Cu-618.
Published: 01 April 2000
..., Inc. Waterbury, CT 06708 (800) 243-3002 (203) 754-0151 (203) 754-1061 (fax) ISSN: 002-614X Cu-618B Table 4 Comparison of Tensile Strength between Phosphor Bronzes and Improved Phosphor Bronzes Tensile strength C51100 WRM 5118 C51000 WRM 5108 C52100 WRM 5218 Temper MPa ksi MPa ksi MPa ksi MPa ksi MPa...
Journal Articles
Alloy Digest (1999) 48 (10): Cu-640.
Published: 01 October 1999
... Comparison of Tensile Strength between Phosphor Bronzes and Improved Phosphor Bronzes Tensile strength, MPa (ksi) Temper C51100 WRM 5118 C51000 WRM 5108 C52100 WRM 5218 C52400 WRM 5248 1 2 hard (H02) 390 483 (55 70) 573 676 (83 98) 400 504 (58 73) 600 704 (87 102) 476 580 (69 84) 656 759 (95 110) 524 628 (76...
Journal Articles
Alloy Digest (1999) 48 (9): Cu-639.
Published: 01 September 1999
... C70260 C42500 C66300 C51100 WRM 4222 Thermal conductivity, W/m · K 169.5 155.7 119.4 107.3 83.7 150.5 Thermal conductivity, Btu/(h · ft · °F) 98 90 69 62 48.4 87 Electrical conductivity, %IACS 40 40 28 25 20 35 Coefficient of thermal expansion, 10 6 / K 17.6 18.0 18.4 17.0 17.8 18.4 Coefficient...