Alloy Digest (1999) 48 (10): Cu-633.
Published: 01 October 1999
... 5078 thermal properties UNS C50780 WRM ALLOY 5078 (Modified Phosphor Bronze) WRM alloy 5078 is a modified phosphor bronze with good electrical conductivity and improved tensile strength and stress relaxation. The patent for this alloy is pending. Chemical Composition, wt Physical Properties...