Alloy Digest (2015) 64 (8): Cu-840.
Published: 01 August 2015
...-resistant alloys elasticity electrical applications fatigue properties heat treatability joinability physical properties tensile properties Wieland-S30 SUPRALLOY workability thermal properties UNS C44750 Wieland-S30 Supralloy is copper alloyed with tin and zinc for parts in the electrical...