Alloy Digest (2014) 63 (6): Cu-831.
Published: 01 June 2014
... or source: Mueller Industries. Producer or Source: Mueller Industries Copyright ┬ę ASM International┬« 2014 2014 ASM International chemical composition hardness machinability MUELLER ALLOY C37000 physical properties tensile properties workability UNS C37000 DATA ON WORLDWIDE METALS...